EI Almen Strips by specification |
| Type "A" (.051") Specification Chart (pdf) |
Electronics Inc. can provide Almen strips to ANY specification, from standard MIL specifications to rigid aerospace specifications.
Almen strips are categorized by thickness, A, N, or C.
See charts for descriptions and pricing. Call for large volume pricing. |
| Type "N" (.031") Specification Chart (pdf) |
| Type "C" (.094") Specification Chart (pdf) |
| |
EI Generic Grade Almen Strips
See descriptions of Grades below.
Call for volume pricing. |
| Type/Grade |
CPN |
Price/Strip |
Quantity/Box |
A-3 |
970045.3 |
$0.65 |
1000 |
A-2 |
970045.2 |
0.81 |
50 |
A-1 |
970045.1 |
1.10 |
50 |
A-1S |
970045.S |
1.25 |
50 |
N-3 |
970047.3 |
0.75 |
1000 |
N-2 |
970047.2 |
0.95 |
50 |
N-1 |
970047.1 |
1.20 |
50 |
N-1S |
970047.S |
1.49 |
50 |
C-3 |
970046.3 |
1.45 |
500 |
C-2 |
970046.2 |
1.70 |
25 |
C-1 |
970046.1 |
2.10 |
25 |
C-1S |
970046.S |
2.50 |
25 |
|
Grade 3 -- bullk
(Meets Mil-S-13165),
Types A-3, N-3, C-3
|
Lowest cost Grade-3 strips are available in type "A", "N", and "C" and are guaranteed to meet the requirement of MIL-S-13165. Type A-3 strip is guaranteed to meet National Stock Number NSN 6635-00-512-1892. |
Grade 2 Standard Grade
(Meets Mil-S-13165):
Types A-2, N-2, C-2
|
Excess oil is removed from the Grade 2 Standard strips. The strip surfaces are then visually inspected for score marks, scratches, nicks, burrs, pits and rust. Strips are certified using a sampling inspection plan for hardness, length, width, thickness, and flatness. A dated certification of compliance is issued, signed and archived. The "A" and "N" strips are packaged in boxes of 50 and "C" strips in boxes of 25. |
Grade 1 Premium Grade
(Meets SAE J442)
Types A-1, N-1, C-1
|
EI performs all the inspection and packaging operations listed for Grade 2 strips. Strips are then sample inspected for flatness (±.001 for A and N strips; ±.0015 for C strips) on each side. A signed and dated certificate of compliance is issued and archived. The Premium Grade 1 strips are identified by a batch control number for traceability. |
Grade 1S Special Grade
(Meets SAE AMS 2432B)
Types A-1S, N-1S, C-1S
|
In addition to requirements for Premium Grade 1, the Grade 1S strips are inspected to ±.0005 flatness tolerance of the Aerospace Materials Specification AMS 2432B. A signed and dated certificate of compliance is issued and archived. |
| *Note: Grades 3,2,1 and 1S are service marks of Electronics Inc. |
High Hardness "A" Strips (packaged 50 per box)
Laboratory grade strips used for very high intensity peening process evaluation. |
| Hardness |
CPN |
Price/ea. |
Material |
Length |
Width |
Thickness |
55 HRc |
999203 |
$4.00 |
SAE 1090 |
3.00 |
.75 |
.051 |
60 HRc |
999204 |
$4.00 |
SAE 1090 |
3.00 |
.75 |
.051 |
AluminumTest Strips (packaged 50 per box) |
| Type |
CPN |
Price/ea. |
Material |
Length |
Width |
Thickness |
| Type W |
970060.W |
call |
7075-T6 |
2.985-3.015 |
.740-.760 |
.151-.155 |
| Type X |
970060.X |
call |
AA2024-T3 |
2.985-3.015 |
.740-.760 |
.123-.127 |
| Type Y |
970060.Y |
call |
AA7075-T6 |
2.985-3.015 |
.740-.760 |
.1545-.1585 |
| Type Z |
970060.Z |
call |
AA7075-T6 |
2.985-3.015 |
.748-.752 |
.139-.141 |
| Aero-Almen |
999202 |
$2.00 |
2024-T3 |
2.94-3.06 |
.745-.755 |
.031-.033 |
| |
Aero-Almen Strips
Used for aircraft paint stripping. For more information see Aircraft Paint Stripping. |