 1987015
Development Of Mechanical Surface Strengthening Processes From The Beginning Until Today
Kloos, K. H. and Macherauch, E.
 1987099
The Responsibility For Reliability
Balcar, G. P.
 1987058
Modern Shot Peening Technology
Nachman, G.
 1987150
About The Influence Of Different Separation Systems On Shot Peening Treatment
Kreikenbaum, H. and Fischer, G.
 1987011
Controlled Shot Peening, Complete Plants And Examples Of Application
Bosshard, R.G. and Hornauer, K.P.
 1987042
Important Considerations For Utilizing Shot Peening As A Design Tool
Simpson, R.S. and Garibay, R.P.
 1987100
The Total Cost of Weight Revisited: An Essay on Cost as a Function of Weight in automobiles and the Use of Shot Peening to R
Terry, S.L. and Simpson, R.S.
 1987101
The Use Of The Shot Peen Process As A Design Tool Through The Use Of Microprocessors
Daly, James J.
 1987005
Automated Shot Peen Quality Control Through The Use Of Parametric Sensors
R. Gillespie, and W. Hasty Jr
 1987095
The Effect Of Inherent Tolerances In The Almen Test Strip On Shot Peening Process Reliability
Simpson, Clark, Chiasson
 1987003
Application Of Shot Peening And Blasting Methods In The Aircraft Industry
Nagel, G.
 1987016
Dovetail Peening By The Deflector Method
Happ, M. B.
 1987055
Maximization Of Flexural Fatigue Strength Of Heat-treated Steel Specimens Using Mult.peen.techniques
Woelfel, M. M.
 1987083
Shot Peening Of Nodular Cast Iron
Parent-Simonin and J Flavenot
 1987087
Shot Peening To Prevent Stress Corr.cracking And Corr.fatigue Failures Of Austenitic Stainless Steel
Risch, K.
 1987010
Controlled Shot Peening Can Help Prevent Stress Corrosion Cracking
Gillespie, B.
 1987088
Shot Peening, Special Application And Procedure
Kiefer, B.
 1987000
Additional Shot Peening For Workshop
Salko, Djosic
 1987044
Improved Fatigue Performance Of Gears Through Controlled Shot Peening
Diepart, C.P. and Burrell, N.K.
 1987097
The Investigation Of Operating Properties Of The Surface After Hammering
Barski, T.
 1987008
Changes In The State Of The Material By Shot Peening
Vohringer, O.
 1987022
Effect Of Work-piece Hardness On Peening Intensity Under Local Peening
Sharma, M. C.
 1987025
Effects Of Plastic Straining On Residual Stresses Induced By Shot-peening
Kirk, D.
 1987108
X-ray Microstructure And Resid.stress Analysis Of Shot Peened Surface Layers During Fatigue Loading
Bergstrom, J. and Ericsson, T.
 1987047
Influence of Change of Microstructure and residual stress field in surface Shot Peen Strain Layer on Fatigue Behavior
Qiu, Q. and Wang, R.
 1987102
Thermal Relaxation Of Shot Peening Resid.stresses In The Diff.heat Treated Plain Carbon Steel Ck 45
Hoffmann, Scholtes, Vohringer
 1987084
Shot Peening Of The Gear Surface With Ground Cracks
Y. Tan, B. Ma, L. Ren, Q. Ye
 1987052
Influence Of The Shot Peening Angle On The Condition Of Near Surface Layers In Materials
Ebenau, Vohringer, Macherauch
 1987103
Topography And Fracture Studies Of Surfaces Shot Peened At Different Intensities
Simpson, R.S. and Probst, R.L.
 1987075
Selected Examples On The Topography Of Shot Peened Metal Surfaces
Kohler, W. and Hornauer, K.-P.
 1987004
Application Of The Incremental Hole Drilling Method For The Measurement Of Residual Stress Distribution In Shot-peened Comp.
Lu, J. and Flavenot, J.F.
 1987081
Shot Peening Of Fast And Electroheated Metals
Al-Obaid, Ismail, Al-Bassam
 1987070
Recent Developments In Shot Peen Forming
Kopp, R. and Ball, H.
 1987077
Shot Peen Forming - An Economical Solution
Tatton, R.J.D.
 1987063
Peen Forming By Pointed Ball Shooting (ball Shot Forming)
Clausen, R. and Bruder, M.
 1987078
Shot Peen-forming Of Nc-machined Parts With Integrated Stringers Using Large Balls
Meyer, Reccius, Schulein
 1987060
On The Effects Of Shot Peen.on The Fatigue Strgth.and The Resid.stresses Of Parts Made Of Ti A16 V4
Kussmaul, Guth, Stuttgart
 1987034
Fundamental Aspects Of The Effect Of Shot Peen.on The Fatigue Strgth.of Metallic Parts And Structure
Lieurade, H.P. and Bignonnet, A.
 1987009
Computer Simulation Of Different Surface Topographies Of Metals Produced By Blasting Processes
Knotek, O. and Elsing, R.
 1987028
Fatigue Behavior Of Shot Peened Steel
Desvignes, Gentil, Khabou
 1987024
Effects Of Peening On Superconducting Transition Properties
Nishi, Harano, Hara, Furukawa, Ninomiya
 1987023
Effects Of Peening On Magnetic Properties In Soft Magnetic Alloys
Nishi, Harano, Kai, Tachi
 1987105
Use Of A Finite Element Meth.for The Prediction Of Shot-peened Resid.stress Relaxation During Fatigu
Lu, J. and Flavenot, J.F.
 1987002
Analysis Of Some Particular Cases Of Shot-peening And Their Influence On Field Of Residual Stresses
Barret, L. and Cailliau, J.
 1987094
Testing Of Shot Blasting Regimes And Metal Prod.surf.hardening Parameters By Barkhausen Effect Meth
Filinov, V. and Shaterniklov, V.
 1987071
Relationship Between Shot Peening Surface Strain Layer And The Fatigue Str. Of High-str.alum.alloy
Renzhi, Xiangbin, Hen
 1987001
An Investigation into the Influence on the Fatigue Strength of Aluminium Alloy Parts of Load Spectrum Base Level and Residual
Jaensson, B. and Magnusson, L.
 1987021
Effect Of Shot-peening On Fatigue And Fretting Fatigue Behaviour Of 8090 And 7010 Aluminum Alloys
Fair, Noble, Waterhouse
 1987061
Optimization Of Shot Peening To Improve The Fatigue Strength Of Ti-6a1-4v
Franz, H.E. and Olbricht, A.
 1987049
Influence Of Shot Peening Induced Surface Roughness, Residual Macrostresses and Dislocation Density on the Elevated Temperatu
Gray, Wagner, Lutjering
 1987020
Effect Of Shot Peening Conditions On Fatigue Strength Of Two Alloys For Turboengines Disks
Guedou, and Evry
 1987018
Effect of Modified Surface Microstructures through Shot Peening and Subsequent Heat Treatment on the Elevated Temperature Fat
Gray, Wagner, Lutjering,
 1987029
Fatigue Behaviour Of Shot Peened Tia16v4 In The Temperature Range 20 Deg.c < T < 450 Deg. C
Hanagarth, Vohringer, Macherauch
 1987092
Study of Fatigue Damage in Shot Peened Aluminium Alloys using Acoustic Emmission and Macro/Microscopic X-Ray Diffraction Inve
Bonnafe, Maeder, Bathias, Compiegne
 1987080
Shot Peening Of Components To Improve Fatigue Strength
Schutz, W.
 1987048
Influence of Peening Parameters, Coating Temperatures and Operating Loads on Residual Stresses of Shot-Peened Barrell Springs
Hutter, W. and Kloos, K.H.
 1987089
Size Effect On Fatigue Strength Of Shot Peened Carburized Steel
Hisamatsu, S. and Kanazawa, T.
 1987098
The Research To The Contact Fatigue Behaviour Influenced by the Residual Stresses on the Surface of the Shot Peened Specimen
Zhu, J. and Guo, P.
 1987046
Improvement To The Fatigue Strength Of Drop-forged Specimens By Airless Blast Cleaning
Kloos, Kaiser, Oppermann
 1987043
Improve Fatigue Limit On Coil Spring
N. Hu, X. Liu, J. Yao and K. Jin
 1987031
Fatigue Strength Of Case Hardened And Shot Peened Gears
Hirsch, Wohlfahrt, Macherauch
 1987069
Practical Aspects of Application of Shot Peening to Improve the Fatigue Behaviour of Metals and Structural Components
Wohlfahrt, H.
 1987085
Shot Peening Of Welded Joints And Residual Stress Relaxation During Fatigue
Bignonnet, Lieurade, Picouet, Castex
 1987050
Influence Of Shot Peening On Fatigue Of Sintered Steels Under Constant And Variable Amplitude Loadng
Sonsino, C.M. and Koch, M.
 1987096
The Effect Of Shot Peening On Fatigue Strength Of Zinc Coated Steels
Burakowski, Nakonieczny, Babul
 1987033
Fatigue Strength Of Work Softening Layer Produced By Shot Peening
Iida, K. and Tosha, K.
 1987086
Shot Peening On Torsion Fatigue
J. He, Y. Wu, Y. Yu, J. Flavenot
 1987073
Residual Stress Concentration And Its Effect On Notch Fatigue Strength
Zhang, K. Xu, X. Wang, N. Hu
 1987051
Influence Of Shot Peening On The Bending Fatigue Behaviour Of Notched Specimens Of Ck 45
Hoffmann, Lohe, Macherauch
 1987062
Optimum Peening Intensities
Fuchs, H. O.
 1987113
Fatigue Progress in Shot-Peened Surface Layers. (Retroactive Coverage).
Berns, H ; Weber, L
 1987053
Investigation On The Effect Of Shot Peening On Elevated Temperature Fatigue Behavior Of Superalloy
Chen, Y. and Wang, R.
 1987032
Fatigue Strength of Shot-Peened Grade 35 NCD 16 Steel. Variation of Residual Stresses Introduced by Shot Peening According to
Bignonnet, A.
 1987026
Effects Of Shot Peening On The Corrosion Fatigue Properties Of Spring Steels
Kaiser, B.
 1987045
Improvement Of Ni 18 (250) Maraging Steel Weldment Fatigue Strength Through Shot Peening
Banas, G. and Lawrence,Jr., F.V.

Note: For additional information go to www.shotpeener.com Jack Champaigne
Last revised on: 01/27/2007

     





HOME | WELCOME | CONTACT US | BUYER'S GUIDE
LIBRARY | ELECTRONICS, INC


©2007 Electronics, Inc. All rights reserved.