ICSP-9 Conference Papers

 2005068
The Interest To Use Tungsten Carbide Balls With Stressonic Ultrasonic Shot-Peening Process: Application To Aero Engines Parts
Jean-Michel Duchazeaubeneix, Sonats
 2005060
Thermo-Elasto-Plastic Model for Shot Peening: A Numerical and Experimental Approach
Rouquette Rouhaud Pron François Bissieux
 2005061
Heterogeneous Ultrasonic Shot Peening: Experiment and Simulation
Micoulaut Retraint Viot François
 2005062
Fundamentals of the Deep Rolling of Compressor Blades for Turbo Aircraft Engines
S Mader, F Klocke
 2005064
Proposing an Applied Information Based Solution in Studying Shot-Peening Process
R Azizi, B Disfani
 2005065
Deep Rolling - The Past, The Present and The Future
I Altenberger
 2005066
Optimization of Residual Stress and Fatigue Life in Laser Peened Componts
MR Hill, TE Pistochini, AT DeWald
 2005069
Effect of Ultra Shot Peening on Contact Surface Strength
Watanabe, Hattori, Handa, Yoshida, Taki, Duchazeau
 2005070
Effect of Deep Rolling at Elevated and Low Temperatures on the Isothermal Fatigue Behavior of AISI 304
I Nikitin, I Altenberger, B Scholtes
 2005071
Deburring and Surface Conditioning of Micro Milled Structures by Abrasive and Non-Abrasive Micro Peening
C Horsch, V Schulze, D Lšhe
 2005072
Shot Peening With Dry Ice
E Uhlmann, M Krieg
 2005073
Cavitation Peening By Using Cavitating Jet In Air
H Soyama, K Homma
 2005074
"Vacuum Blasting". An Innovative New Process For Metallic Coating Of Surfaces With A Shot / Powder Mixture
Gerard Pieper, Sigurd Ruhland
 2005075
Optimisation of Carburising and Shot Peening, In Order To Improve Both Bending and Contact Fatigue Behaviour For Gear Applica
C Peyrac, J Flavenot
 2005089
Fatigue Limits Prediction of Shot Peened Materials
H. Guechichi*, L. Castex**
 2005090
Fatigue Strength Prediction of a Shot Peened 42CRMO4 Steel Using Multiaxial Fatigue Criterion and Surface Roughness Correctio
Palin-Luc, Flavenot, Lasserre, Charles, Leguernic
 2005091
Residual Stress Sensitivity of Case-Hardened Notched Specimen
Krug, Lang, Lšhe
 2005092
The Effects of Shot Peening and Deep Rolling on the Surface Layer and the Mechanical Properties of Sintered Iron
Merkel, Schulze, Všhringer
 2005093
Comparison of Mechanical Suppression by Shot Peening and Low Plasticity Burnishing to Mitigate SCC and Corrosion Fatigue Fail
Prevey, Jayaraman, Ontko, Shepard, Ware, Coate
 2005094
Static and Dynamic Strain Ageing of Deep Rolled Plain Carbon Steel SAE 1045 for Optimized Fatigue Strength
Altenberger, Nikitin, Scholtes
 2005095
Fatigue Life Improvement Through Nanostructuring of Stainless Steel
Roland, Retraint, K Lu, J Lu
 2005096
Overview of Low Plasticity Burnishing for Mitigation of Fatigue Damage Mechanisms
Prevey, Jayaraman, Cammett
 2005097
Analysis of the Influence of Shot Peening on the Fatigue Life of a Hard Chromium Electroplated AISI 4340 Steel Underplate
Torres, Baptista, Nascimento, Voorwald
 2005098
Fatigue Strength of the Steel After the Percussive Burnishing Process
D. Stadnicka
 2005099
Fatigue Performance of Light-Weight Alloys: Influences of Shot Peening and Pre-Corrosion
C. Mueller and L. Wagner
 2005100
Coverage Effects in Shot Peening of AL 2024-T4
T. Ludian and L. Wagner
 2005101
Effect of Deep Rolling on the Fatigue Behavior of Under-, Peak- and Over-Aged AA6110 at Room Temperature
P. Juijerm, I. Altenberger, B. Scholtes
 2005102
Mechanical Surface Treatments on the High-Strength Wrought Magnesium Alloy AZ80
Zhang, Lindemann, Kiefer and Leyens
 2005103
Deep Rolling of Titanium Rods for Application in Total Hip Arthroplasty
Eigenmann, Holzwarth, Kachler, Gšske, Wilcke, Schu
 2005104
Effects of Aging Treatment and Shot Peening Variables of HCF Performance of Timetal LCB
Kocan, Rack, Wagner
 2005106
Effect of Prior Cold Work on Fatigue Performance of Shot Peened TI-2.5CU
H. Boeckels and L. Wagner
 2005105
Advances in Shot Peening of Silicon Nitride Ceramics
W. Pfeiffer and T. Frey
 2005107
Effects of Shot Peening on the Corrosion Fatigue Life of Al 7075-T6
Cheong, Nam, Lee, Kim
 2005108
Evolution of Shot Peening Experimental Techniques
D. Kirk
 2005109
History of Shot Peening Specifications
J. Champaigne
 2005110
Implementing On-Line Process Control for Shot Peening
Haubold, Hennig, WŸstefeld, Kittel, Friese
 2005111
On-Line Process Control for Shot Peening Applications
WŸstefeld, Linnemann, Kittel, Friese
 2005112
Relationship Between Coverage and Surface Residual Stress
D. Kirk and R. C. Hollyoak
 2005113
Influence of Shot Velocity and Shot Size On Almen Intensity and Residual Stress Depth Distributions
W. Zinn and B. Scholtes
 2005114
Particle Velocity Sensor for Improving Shot Peening Process Control
Barker, Young, Pouliot
 2005115
Factors That Influence Almen Strip Arc Height
P. Bailey and J. Champaigne
 2005116
Shot Peening and Grit Blasting - Effects on Surface Integrity-
Tosha, Lu, Guelorget, Nagashima
 2005117
Optimising Shot Peening Parameters Using DoE
Lassithiotakis, Aylott, Shaw, Ooi, Petit-Renaud
 2005118
Characterization of Shot Peened Components by X-Ray Diffraction: A Method On Its Way From the Laboratory Into Industrial Prod
Wulf Pfeiffer
 2005119
Stability of Surface Changes Induced By Mechanical Surface Treatments
V. Schulze
 2005120
The Effect of Shot Peening Coverage on Residual Stress, Cold Work and Fatigue in a Nickel-Base Superalloy
J. Cammett, P. Prevéy and N. Jayaraman
 2005121
Evolution of the Residual Stresses by Stress Rolling
Eckehard MŸller
 2005122
Eigenstrain Generated by Shot Peening in Udimet 720LI Inferred By Means of Finite Element and Analytical Models
M. Satraki, A. Evans, A. King, G. Bruno, P. Wither
 2005123
Effect of Shot-Peening on the Fatigue Strength of Spring Steel After Exposure to Corrosion
A. Nakonieczny and G. Monka
 2005124
The Effect of Incidence Angle on Residual Stress State In Laser Peened Ti-6Al-4V Plate
Evans, King, Pirling, Bruno, Withers
 2005125
Relation Between Microstructure of Shot-Peening Steel And Its Mechanical Characteristics
Haga, Harada, Tsubakino
 2005126
Laser Shock Processing As A Method For Surface Properties Modification Of Metallic Materials
Oca–a, Morales, Molpeceres, Porro
 2005127
Characteristics of Internal Surface Layer of Machine Parts Using Rebound Shots
Yasunori Harada
 2005054
Effect of Metal-Spraying and Shot Peening on Abrasive Wear of Carbon Steel
MC Sharma, SC Modi
 2005055
Finite Element Analysis of Shot Peening -On the Form of a Single Dent-
N Hirai, K Tosha, E Rouhaud
 2005056
A 3-D Numerical Study of Shot Peening Process Using Multiple Shot Impacts
GH Majzoobi , R Azizi
 2005063
Calculated Determination of Optimum Peening Conditions In Terms of Collision Energy on Coil Spring by Shot Peening
A Amano, T Sakakibara, M Wakita, Chuo Spring Co Lt
 2005067
Generation of Nanostructures by SMAT
Jian Lu, K. Lu

 

     