How Shot Peening Makes Better Gears
Author: Cary
Source: American Gear Mfrs. Assoc,. Nov., 1973
Doc ID: 1973007
Year of Publication: 1973
Abstract:
Descriptors: Carbon steels-- Surface finishing; Chromium molybdenum steels-- Surface finishing; Shot peening; Strain hardening; Gears-- Surface finishing