Measurement Of Stresses Induced By Shot Peening

Author:  Birley, S.S. and Owens, A.
Source:  Conf Proc: ICSP-1, (p.249-254)
Doc ID:  1981049
Year of Publication:  1981
Abstract:  
The stress state induced by shot peening is a measure of the quality of the peening process. The center hole drilling technique is described and compared with X-ray techniques for stress analysis of A1 alloys. Descriptors: Aluminum base alloys-- Mechanical properties; Shot peening; Stress anaysis; Strain gages; X ray diffraction