Effects Of Multiple Shot Peening/cadmium Plating Cycles On High Strength Steel
Author: Kohls, Cammett, Gunder
Source: Metcut Research Assoc., Inc.
Doc ID: 1982005
Year of Publication: 1982
Abstract:
A study was made of the effects of multiple shot-peening and Cd plating operations on high-strength AISI 4340 steel used in aircraft landing-gear applications. No detrimental effects were observed on surface microstructure and tensile properties or on fatigue and unnotched stress corrosion resistance in high-humidity air. An apparent degradation in stress corrosion life of fatigue precracked specimens was observed after four and five peening and plating operations.
Descriptors: Nickel chromium molybdenum steels-- Mechanical properties; Cadmium plating; Shot peening; Tensile properties; Landing gear; Fatigue (materials); Stress corrosion cracking