A New Method of Measurement of the Velocity of Solid Particles and Their Mass For Air Blasting

Author:  J Andziak
Source:  Conf Proc: ICSP-7 (pg 308-312)
Doc ID:  1999042
Year of Publication:  1999
Abstract:  
The results of air blasting are presented. The methods of measurement of velocity of solid particles are characterized. The new, original threefold - disk method of measurement of the velocity and mass of solid particles is described as well as construction of the measureing instrument.