Influence Of Shot Peening And Burnishing On Smooth And Notched Fatigue Strengths Of Titanium Alloys

Author:  T. Ludian, J. Atoura and L. Wagner
Source:  Conf Proc: ICSP-10 Tokyo, Japan 2008
Doc ID:  2008097
Year of Publication:  2008
Abstract:  
ABSTRACT The high cycle fatigue (HCF) response to shot peening (SP) and ball-burnishing (BB) of two titanium alloys - one belonging to the