Rotary Flap Peening of Metal Parts

Author:  SAE
Source:  SAE: AMS2590 Issued 2010-12
Doc ID:  2010034
Year of Publication:  2010
Abstract:  
This is a new specification that provides technical improvements to MIL-R-81841 in these areas: (1) two methods for determination of intensity independent of peening time, (2) improved operator qualification requirements, (3) more effective methods for determination of peening time, and (4) simplified calculation of required tool speeds within holes.