Patent Application Publication Aluminum fan Blade Root
Author: Watson, Pasakarnis, Cowles, Smith
Source: U.S. Patent Office
Doc ID: 2013002
Year of Publication: 2013
Abstract:
A method of improving fatigue strength in a fan blade includes fabricating a metal fan blade with an airfoil and a root and deep peening the root.