Title: Shot Peening - Designers Guide to the Process, its Applications
Author: Fuchs, H.O. and Hutchinson, E.R.
Source: Machine Design, Vol. 30, Feb. 6, '58, pp. 116-125
Publication year 1948
Document number: 1948013
Number of pages: 10
Abstract:
Developed in the late twenties, shot peening was discovered by accident. a small batch of automobile valve springs behaved much better than expected under test.
Investigation revealed that thet had been shot blasted to improve the surface. this discovery led to commercial development of the process, although up to the start of the
second world war the process was confined almost exclusively to automotive parts such as springs, gears and axles. During the war, pressing need for higher performance
without increased weight caused rapid development of the shot peening process.