Title: How, When And By Whom Was Mechanical Prestressing Discovered
Author: Bush and Almen, Danse and Heiss
Source: SAE Division XX Presentation
Publication year 1962
Document number: 1962003
Number of pages: 11

Abstract:
in collaboration with J. O. Almen, L. A. Danse and J. P. Heiss Prestressing of metals by mechanical working to obtain improved strength and fatigue characterisitics has been developed gradually over many years.