Title: Shot Peening - Theory
Author: Straub, J.
Source: AMGA Meeting, May, 1962
Publication year 1962
Document number: 1962005
Number of pages: 7

Abstract:
Shot peening differs from blast cleaning, mainly in its purpose. the most common purpose of peening is to accomplish an increase in fatigue strength. The question is often asked, "how much increase can be expected?" It is easy to cite examples of increased fatigue life in specific cases because there are so many case histories to refer to.