Title: Process Specification for Shot Peening of Metal Parts
Author: General Dynamics
Source: FPS-1032
Publication year 1963
Document number: 1963010
Number of pages: 13

Abstract:
This specification establishes requirements for shot peening of steel and aluminum alloy parts. Shot peening in accordance with this specification is intended to be used to impose compressive stresses on the specified surgaces to increase fatigue strength and/or to prevent stress corrosion.