Electronics Incorporated - The Shot Peener - Shot Peening Library


Title: Aircraft Accident Report NTSB File 1-0016, Los Angels Airways Inc, S-61L Helicopter N300Y August 14, 1968
Author: National Transportation Safety board
Source: National Transportation Safety Board
Publication year 1969
Document number: 1969049
Number of pages: 18

Abstract:
Los Angeles Airways, Inc, S-61L helicopter, N300Y, crashed at Compton, Californina, on August 14, 1968, at approximately 1035 PDT. All 18 passengers and three crewmembers were fatally injured, and the aircraft was destroyed by impact and fire. The Safety Board determines that the probable cause of this accident was the fatigue failure of the main rotor blade spindle, causing separation of the blade which made the aircraft uncontrollable. The fatigue crack originated in an area of substandard hardness and inadequate shot peening.