Title: Shot Peening Of Steel, Aluminum, And Titanium Parts
Author: Bell Helicopter Textron
Source: BPS 4409 Dec 21,1979
Publication year 1979
Document number: 1979006
Number of pages: 22

Abstract:
This specification outlines the requirements for the materials, equipment and procedure to be used in the shot peening of steel, aluminum, and titanium parts.