Abstract:
The resistance of high-strength carbon-steel wires to hydrogen cracking due to corrosion by seawater containing hydrogen sulfide is largely improved by shot-peening.
Descriptors: Corrosion sous tension; Acier au carbone a haute caracteristique mecanique; Eau de mer; Hydrogene sulfure; Grenaillage de precontrainte