Title: Contribution A L'etude Du Parachevement Des Soudures Pour L'amelioration De Leur Resist.a La Fatigue
Author: Bramat, M.
Source: Conf Proc: ICSP-1, (p. 71-82)
Publication year 1981
Document number: 1981014
Number of pages: 10
Abstract:
The objective of weld treatments to increase the fatigue limit of the assemblies is to create more favorable microstructures and residual stresses. Results are given of a
study on steel E36-3 of the improvements as a result of Tig remelting of the weld toe, peening between passes, peening of the last run and prestressing by shot peening. It
appeared that shot peening and hammer peening were the most efficient techniques.
Descriptors: Structural steels-- Welding; Gas tungsten arc welding; Welded joints-- Mechanical properties; Fatigue strength; Shot peening; Prestessing