Title: Control Of Stress Corrosion Cracking By Shot Peening
Author: Takemoto, Shinohara, Shirai
Source: Conf Proc: ICSP-1, (p.521-528)
Publication year 1981
Document number: 1981015
Number of pages: 7
Abstract:
Studies were carried out to determine the protective effects of shot peening sgainst stress corrosion cracking (SCC) of austenitic stainless steel 304. SCC susceptibility
of shot-peened specimens was evaluated by using a constant load type SCC test apparatus in three kinds of corrodents. Beneficial effects and some problems encountered in
shot peening for the prevention of SCC are discussed.
Descriptors: Austenitic stainless steels-- Corrosion; Stress corrosion cracking; Shot peening; Chlorides-- Environment; Corrosion prevention