Title: Measure And Control Of Impact Finishing Processes
Author: Neelakantan, Green, Foo, John
Source: Conf Proc: ICSP-1, (p.147-158)
Publication year 1981
Document number: 1981046
Number of pages: 12
Abstract:
A system of monitoring and regulating the shot-peening intensity of a nozzle-type peening machine has been designed. The over-all aim is a machine capable of producing a
required change in surface finish and strength by measuring both the kinetic energy of the shot-peening material and the peening time. Two measuring systems are outlined
and detailed results are presented for the lower-cost system.
Descriptors: Shot peening; Monitoring; Nozzles; Measurement; Computer programs