Abstract:
The effects of shot-peening on the elevated temperature fatigue properties (550-800oC) of four iron base, four wrought nickel base and one cast nickel base superalloys were investigated. It was found that the elevated temperature fatigue strength of all suepralloys can be improved by shot-peening in different degree, and the effects of fatigue improvement are more pronounced for notched specimens. Descriptors: Shot-peening, Elevated temperature fatigue (superalloys); Subgrain; Latticedistortion; Residual stress; Fractography