Abstract:
The effect of shot peening and surface rolling on fatigue strength of a medium carbon chromium steel at different heat treated conditions was investigated and emphatically
discussed from the changes in residual stresses, structure and fractographic morphology.
Descriptors: Surface plastic deformation; Fatigue strength; Residual stresses; Structural and fractographic changes