Title: An Engineering Approach To Shot Peening Mechanics
Author: Al-Hassani, S.T.S.
Source: Conf Proc: ICSP-2, (p.275-282)
Publication year 1984
Document number: 1984001
Number of pages: 8

Abstract:
A simple theoretical analysis of the shot peening process is presented. The process is viewed as one involving multiple and progressively repeated impact. The residual stress field under each impact interacts with similarly produced neighbouring fields to finally produce a residual stress distribution varying in depth but uniform in planes, parallel to the surface. Non-dimensional numbers which are useful for similarity considerations are introduced. New concepts such as shakedown, reversed plastic yielding and Bauschinger effect as well as strain rate are thought to contribute a significant role in the process. Descriptors: Analysis; Residual stress distribution; Arc height; shakedown; Nondimensional numbers


Download full text pdf file

www.shotpeener.com
This page last revised: 03/04/2009
spc2003a.frx