Title: An Overview Of Peen Forming Technology
Author: Baughman, D.L.
Source: Conf Proc: ICSP-2, (p. 28-32)
Publication year 1984
Document number: 1984003
Number of pages: 6
Abstract:
Curving aircraft skins by the peen forming process has replaced traditional forming methods on many aircraft types. The process has facilitated major advances in aircraft
manufacturing technology. This paper describes application techniques, process variables, limitations, applicable machine designs, and aircraft design considerations that
facilitate peen forming
Descriptors: Wings (aircraft); Sheet metal-- Metal working; Aluminum base alloys-- Metal working; Shaping; Shot peening