Title: Behavior Of Peen-formed Steel Strip On Isochronal Annealing
Author: Kirk, D.
Source: Conf Proc: ICSP-2, (p.231-236)
Publication year 1984
Document number: 1984004
Number of pages: 6
Abstract:
X-ray residual stress measurements and precision curvature measurements were made on rectangular steel strips that had been peen-formed and then subjected to different
isochronal annealing treatments. The initial surface residual stress and curvature levels were substantially greater for the transverse than for the longitudinal direction.
Relief of both curvature and residual stress occurred that increased with temperature up to 400 Deg C. No further relief was observed above this temperature. The relief of
curvature reached 52% for the transverse direction and 40% for the longitudinal direction as compared to more than 95% of the residual stress. An anomalous effect was found
for annealing at 425 Deg C.
Descriptors: Peen-forming; Residual stress, Isochronal annealing; Stress relief