Title: Kugelstrahlumformen, Neuere Technologische Und Theoretische Entwicklungen
Author: Kopp, R. Prof.
Source: Conf Proc: ICSP-2, (p. 6-14)
Publication year 1984
Document number: 1984042
Number of pages: 9
Abstract:
Shot-peenforming and shape-punch-forming combined with elastic prestraining are methods to form large integrally stiffened panels with very different wall thicknesses. A
theoretical model based on the plastic flow of material shows how to calculate the curvature.
Descriptors: Shape of tools; Elastic prestraining; Forming strategy; Curvature of sheet parts; Modeling; Forming process control