Title: The Influence Of Peening Conditions On The Resulting Distribution Of Residual Stress
Author: Wohlfahrt, H.
Source: Conf Proc: ICSP-2, (p.316-331)
Publication year 1984
Document number: 1984068
Number of pages: 16
Abstract:
A concept is presented which is capable to explain numerous different residual stress distributions after shot peening. The concept is based on two competitive residual
stress generating processes. The influence of shot peening conditions on the distribution of residual stresses is discussed in accordance with this concept.
Descriptors: Shot peening; Residual stress; Plastic deformation; Hertzian pressure; Strain hardening; Surface roughness; Hard shot; Glass beads; Steels; Aluminium alloys;
Titanium alloys