Title: The Relationship Between Peening Intensity And Metal Erosion Rate With Respect To Nozzle Angle
Author: Farrari, V.A. and Woelfel, M.M.
Source: Conf Proc: ICSP-2, (p.269-270)
Publication year 1984
Document number: 1984069
Number of pages: 2
Abstract:
Metal erosion is related to nozzle angle when peening with glass beads. Data is presented to show that metal erosion is greatest at or near 90 Deg nozzle angles and that
surface finish is largely independent of nozzle angle when peening pressure is held constant.
Descriptors: Shot peening; Surface finish; Metal erosion; Glass beads