Damage of operating highly loaded parts of turboengines, especially disks, is mainly due to flight cycles "take off-cruise-landing", which are cause of low cycle fatigue
phenomena, with high stress-strain amplitude and low frequency. Therefore, it is very important to improve as much as possible the fatigue strength of those components, and
surface conditioning is an outstanding parameter which greatly influences the fatigue life. A widely used industrial process for surface condition enhancement is shot
peening, which is known to have effect both on mechanical properties and on surface microgeometry. Thus in order to determine the optimized conditions of shot peening on
disks alloys a study of various shot peening parameters has been carried on concerning laboratory test specimens of two disks materials: a titanium and a nickel based
alloys.