Title: Effects Of Peening On Superconducting Transition Properties
Author: Nishi, Harano, Hara, Furukawa, Ninomiya
Source: Conf Proc: ICSP-3, (p.377-382)
Publication year 1987
Document number: 1987024
Number of pages: 6
Abstract:
A peening generates lattice defects and a compressive stress without a large quantity of deformation. Tc often changes the lattice constant which is varied by the defects,
such as a constitutional vacancy, and a solute concentration of A-15 phases. Since the constant is dominated by the defects and the stress, the peening may be a good tool
to increase Tc. However, it is difficult to peen most of A-15 chemical compounds because of their fragility. Besides high superconducting transition temperatures, the
liquid-quenched Nb-A1 alloys (mixture of A-15 + bcc) show ductility. The purpose of the present work is to investigate the effects of the peening on Tc of Nb(3)A1
crystalline alloys prepared by the liquid-quenching.