Abstract:
We have come to the third gathering of the world community of the art, science and practice of shot peening to share our work and our mutual fascination with this great phenomenon. The manipulation of surface stresses of metals has great prospects of service to the world society. Each one of us has personal contributions in mind to making one or several of those prospective benefits come to pass.