Title: The Use Of The Shot Peen Process As A Design Tool Through The Use Of Microprocessors
Author: Daly, James J.
Source: Conf Proc: ICSP-3, (p. 87-91)
Publication year 1987
Document number: 1987101
Number of pages: 5
Abstract:
An abundance of data has been presented and recorded over the last 40 years on the benefits of mechanically prestressing components which are subject to a metal fatigue as
well as stress corrosion cracking. The most flexible and inexpensive method has broven to be the shot peening process. However, prior to the advent of sophisticated sensors
and computers, lack of precise control over the process has not allowed the design engineer to take credit for the use of the process in his original design calculations.