Abstract:
This specification establishes the requirements for shot peening relatively small areas of metal surfaces, including holes, for the purpose of imparting a compressive layer. T he techniques employed contain the shot on the tool and prevent contamination of the surrounding area with loose shot. B AC 5730 forms a part of this specificaiton only to the extent indicated herein.