Title: Shot Peening Process Specification Departure 6-61 (BAC 5730)
Author: Boeing Commercial Airplane Co.
Source: BAC 5730 (6-61)
Publication year 1988
Document number: 1988064
Number of pages: 1

Abstract:
To allow glass bead peening as an optional secondary peening operation to improve surface roughness.