Title: Metal Improvement Company: Review of Shot Peening Technology
Author:
Source: Impact: Fall 1989
Publication year 1989
Document number: 1989060
Number of pages: 4

Abstract:
IN THIS ISSUE: 1) Stress Corrosion Cracking: Prevention and Cure 2) Henry Fuchs Dale R. McIntyre, formerly with Battelle-Houston, wrote: Stainless steels as a class offer the chemical engineer many attractive features: good corrosion resistance, weldability, fabricability and reasonable cost. However, any engineer hoping to take advantage of these benefits must consider the possibility of stress-corroion cracking.