Title: Steel Shot Peening For Improved Fatigue, Stress Corrosion And Fretting Resistance
Author: British Aerospace
Source: BAEP 2009 Issue 1
Publication year 1990
Document number: 1990079
Number of pages: 21

Abstract:
This specification covers procedure requirements for automated steel shot peening of steel, titanium and aluminium alloys. The purpose of shot peening is to induce residual compressive stresses in specified surfaces thus increasing the fatigue strength and resistance to stress corrosion cracking and fretting.