Abstract:
Bending fatigue tests were carried out on smooth and notched (stress concentration coefficient Kt=1.5 and 3.0) specimens of 40Cr steel to determine the fatigue strength for
5X10 6 by up and down method. The specimens were shot peened and ground after heat treatment (quenched and tempered at 200C and 550C). Special attentions were paid to
determined the positions of crack sources to subsurface and results in higher improvement in fatigue strength. The apparent fatigue strength of notched specimens tempered at
550C even reaches that of the crack source after shot peening still initiates at the root of the notch from the surface and the improvement of fatigue strength is not so
significant as in above case.