Title: Theoretical Basis of Shot Peening Coverage Control
Author: D. Kirk and M.Y. Abyaneh
Source: Conf Proc: ICSP-5, (p.175-183)
Publication year 1993
Document number: 1993071
Number of pages: 8
Abstract:
A simplified treatment of the theoretical basis of coverage control is presented based on the application of an Avrami equation. This application shows how coverage
progresses during shot peening with a necessary exponential approach
to 100%. The effects of varying the common shot peening parameters - shot size, peening rate and exposure time are analysed.