Title: Shot Peening Process Specification Departure 9-1 (BAC 5728)
Author: Boeing Commercial Airplane Co.
Source: BAC 5728 (9-1)
Publication year 1993
Document number: 1993102
Number of pages: 1

Abstract:
To increase the chromium contamination limit of Niposit 65 plating bath to 40 PPM maximum.