Electronics Incorporated - The Shot Peener - Shot Peening Library


Title: 01-01-13
Author: Airbus Industrie
Source: Airbus Industrie
Publication year 1993
Document number: 1993145
Number of pages: 17

Abstract:
This document outlines the requirements and defines the necessary operations for shot peening metallic parts. All details of the process shall be recorded on a "component specific instruction" which contains the requirements of the Design Authority. The "component specific instruction" shall be approved by the Design Authority before this process is used.