Title: Simulation of Residual Stress Distribution on Shot Peening
Author: Y. Watanabe, N. Hasegawa
Source: Conf Proc: ICSP-6, (p.530-535)
Publication year 1996
Document number: 1996037
Number of pages: 6
Abstract:
The present research aims at obtaining a theoretical solution on basis of actural measurements of residual stress by shot peening. Firstly, it was conducted that residual
stress on two different strength of plate specimens have been shot peened are measured by X-ray difractometer and the effect of a few type of shot peening conditions on
profiles are confirmed. The equation to simulate profiles was obtained by the superpostition method of simple three stress, based on the equation that Y.F.Al-Obaid
suggested.
It was confirmed that the predicted stress profile shows good correspondence with experimental value in case of every shot peening conditions in this study.