Title: Developments in Interactive Control of Shot Peening Intensity
Author: David Kirk
Source: Conf Proc: ICSP-6, (p. 95-106)
Publication year 1996
Document number: 1996056
Number of pages: 12
Abstract:
Interactive control of shot peening is based on continuous monitoring of peening intensity changes. The latest development in monitoring presented here involves the use of
an elastically-strained arm carring a strain guage that is in contact with a disposable steel disc. As the disc deforms, due to peening, the arm relaxes with consequent
strain guage signal changes being continuously chart-recorded. The divice has been used to study the effects of peening distance, air pressure and peened area on peening
intensity/peening time changes. The very high sinsitivity of the strain guage device allows very small changes in intensity to be detected.