Title: Residual Stresses in Plastically Deformed Wires
Author: Fryderyk Knap
Source: Wire Journal International Publication
Publication year 1998
Document number: 1998007
Number of pages: 5
Abstract:
Wire and wire-based products comprise the majority in the group of plastically deformed steel products. Often those products work at high external loads. Ropes and cords
in lifting equipment, all kinds of springs, cord to reinforce tires, various kinds of strings, wire to reinforce concrete and other wire products can be included in this
category. Behavior of various machine and construction elements and reliability of their operation which guarantee steady and safe fowrk depend mostly on an external layer
condition. Residual stress in one of the most substantial parameters that determine the external layer condition.