Title: Shot Peening for inducement of compressive surface stresses for metal parts
Author: Bureau de normalisation de L'Aeronautique et de lE
Source: Bureau de normalisation de L'Aeronautique et de lE
Publication year 1998
Document number: 1998017
Number of pages: 20

Abstract:
The purpose of this standard is on one hand to specify the donditions under which the shot peening to induce compressive surface sttresses must be carried out, as well as the equipment and technique to be used, and on the other hand to specify the measures to be taken and the operations to be carried out to test the prestressing shot peening operation.