Abstract:
Reprinted with permission 1997 Automotive Engineering Magazine - July 1997 Society of Automotive Engineers, Inc.
Fatigue expectations traditionally have been formulated during the experimental stage of product development to evaluate unexpected failures seen in proving-ground vehicle
testing or to define procedures for accelerated laboratory bench tests. A key feature of the modern durability design process is integration of computing methods with
finite-element analysis (FEA) to predict durability early in design. In the automotive industry, early evaluation of fatigue performance can increase reliability and reduce
product development time.