Title: The Temperature Change on Surface of Workpiece During Peening
Author: N. Hasegawa, K. Hattori, Y. Watanabe, K. Fukuyama
Source: Conf Proc: ICSP-7 (pg 54-59)
Publication year 1999
Document number: 1999015
Number of pages: 5
Abstract:
A study has been made to investigate the temperature change on surface of specimen using a thermograph during shot peening. It was confirmed that the temperature change of
annealed specimens is greater than that of carburized specimens, as well as an occurence of temperature ascent when peening with smaller shot. However, the softened
smallest shot experienced only slight temperature changes. This change was caused mainly by abrasion.