Abstract:
This paper reports the results obtained from a numerical simulation using the Finite Element Method of three cases of shot peening: 1) single shot impacts normal to the target with three different impact velocities; 2) a five shot successive series of normal impacts along a line and overlap, causing ovalisation of the indentation; 3) a single shot impact at an oblique angle to the peened surface. In the analyses the material was considered to exhibit linear-elastic behaviour with a non-linear work hardening characteristic, and a strain rate dependency. The shakedown effect is a natural consequence of the material elastic plastic model behaviour used in this solution procedure. Several other important features associated with material strain-rate dependency and work hardening, hitherto unreported in the literature, are observed and discussed in detail. Possible explanations of the results are presented.


Download full text pdf file

www.shotpeener.com
This page last revised: 03/04/2009
spc2003a.frx