Title: Stability of Residual Stresses in Shot Peened & High Pressure Water Peened Stainless Steels at Elevated Temperatures
Author: P Krull, Th Nitschke-Pagel, H Wohlfahrt
Source: Conf Proc: ICSP-7 (extra)
Publication year 1999
Document number: 1999064
Number of pages: 10
Abstract:
In water surrounded areas many failures of stainless steels are caused by stress corrosion cracking. If the surface of these materials is changed by peening processes,
compressive residual stresses will be induced and stress corrosion cracking may not occur. For this reason stainless steel of type 316 Ti (1.4571) was shot peened and also
high pressure water peened to induce compressive residual stresses in surface layers. During normal service conditions the strain hardened surface layers have been exposed
to elevated temperatures. The influence of time and different temperatures on the stability of residual stresses in surface layers were investigated. The relaxation of the
residual stresses at the surface and in near surface areas was measured by means of X-ray diffraction. With the presented experimental results the effects of peening
processes can be evaluated with respect to typical thermal loading effects.