Title: Calibration of Vibration Shot Peening Fatique Life and Limit Residual Stresses After Technological Process
Author: Salko Djozic, B.Sc.
Source: Conf Proc: ICSP-7 (pg 359-361)
Publication year 1999
Document number: 1999069
Number of pages: 3
Abstract:
Wohlers curve shows us behaviour of steel materials under permanent loading, resistance of material Knowledge, that the Shot Peening helps and saves material from the
residual stresses. Fatique of material must be under checking. Causes of fatique can be different but vibrations must not have value for decreasing mechanical properties.
Speaking in general Shot Peening increasing fatique stresses and higher qualitiy is evidented - improvement in the fatique limit if is following Wohlers diagram. Same thing
is in HOOK'S LOW - betterment of mechanical properties.