Title: Method for Producing a Diaphragm Spring
Author: Hiroshi Mizukami, Neyagawa, Japan
Source: US Patent 5,868,022
Publication year 1999
Document number: 1999076
Number of pages: 7

Abstract:
The invention relates to a method for producing a diaphragm spring where only specific portions of the diaphragm spring are subjected to a shot-peening process. The shot-peening step is performed only to one side of an outer circumferential portion and an inner circumferential portion of the elastic portion (5a) of the diaphragm spring (5).